XLVIII .
The Method of making Sal Ammoniac in Egypt ; as communicated by Dr. Linnaeus , from his Pupil Dr. Hasselquist , who had been lately in those Parts : By John Ellis , Esq ; F. R. S. SAL Ammoniac is made from the soot arising from the burnt dung of fourfooted animals , that feed only on vegetables .
Read Jan. 31 , 1760 .
This dung is collected in the four first months of the year , when all their cattle , such as oxen , cows , buffaloes , camels , sheep , goats , horses , and asses , feed on fresh spring grass , which , in Egypt , is a kind of trefoil , or clover : for when they are obliged to feed their cattle on hay , and their camels on bruised date kernels , their excrements are not fit for this purpose ; but when they feed on grass , the poor people of Egypt are very careful to collect the dung quite fresh , and , for that purpose , follow the cattle all day long , in order to collect it as it falls from them ; and , if it is too moist , they mix it with chaff , stubble , short straw , or dust , and make it up in the form of cakes , about the same size and shape as it lies on the ground .
Philos. Trans. Vol. LI .
TAB. XI .
p. 505 .
A Plan of the subliming Jurnace or Oven for making ~ Ammoniac in Egypt taken from the desoription here given .
Then they fix it to a wall to dry , till it is fit to be burnt .
For want of wood , which none but the rich in Egypt can afford to buy , they burn this dung through the whole country , and sell a vast quantity of it to the salt-makers .
The excrements of the camel are not found at all preferable to any other ; and its urine is never used for this purpose , although generally reported so by authors .
The salt-workers pretend , that the human excrements , and those of goats and sheep , are preferable to any other .
The months of March and April is the only time they make the salt .
Sal ammoniac is made in the following manner : They build an oblong oven , about as long again as broad , of brick and moist dung , of such a size , that the outside , or flat part of the top of the arch , may hold fifty glass vessels , ten in length , and five in breadth , each vessel having a cavity left for it in the brick-work of the arch .
See Tab. XI .
These glass vessels are globular , with a neck an inch long , and two inches wide .
These vessels are of different sizes , in different saltworks , containing from a gallon to two gallons ; but , in general , are about 18 inches diameter .
They coat each vessel over with a fine clay ( which they find in the Nile ) , and afterwards with straw ; they then fill them two-thirds full of soot , and put them into their holes on the top of the oven .
They make the fire gentle at first , and use the aforementioned dried dung for the fuel ; they increase crease the heat gradually , till they bring it to the highest degree , which the workmen call hell-fire , and continue it so for three days and three nights together .
When the heat is come to its due degree , the smoke shows itself , with a sourish smell , that is not unpleasant ; and , in a little time , the salt sticks to the glasses , and covers the whole opening .
The salt continues subliming , till the above-mentioned time is expired ; then they break the glasses , and take out the salt , just in the same form , and of the same substance , that it is sent all over Europe .
At each salt-work , they have a glass furnace , to melt the old glasses , and make new ones .